Silicon dioxide (1600)
Silicon dioxide (1600)
Silicon dioxide (1600)

Silicon dioxide (1600)

$120.82
Model:
MA-EN-AN-0027
item_No
Specifications
Price
MA-EN-AN-002701
Silicous oxide (1600) 20g
$120.82

Details

The material needs to be sealed and stored

It is recommended to use carbon coated copper foil for half cell testing

The electrolyte used during testing is NCM electrolyte (KLD-1230C)

Baking conditions for electrode: Bake at 85 ℃ for 4 hours

Lithium ion anode electrode material, coated with carbon by CVD, with a reversible capacity of up to 1600mAh/g for the first time.

Physical and chemical properties

image.png

Half battery test

bcf69580723ace99a4b83193094e76c.jpg

cec8fe175c9a72c6bf3b5a32b001336.jpg

d0f9282a792b4e954d52c82cdd27a5b.jpg

a86fcc67e6ad409323e42ce808f5cd4.jpg

DC rate discharge, CC rate charging