MA-EN-CA-008801
20g
$45.31

Details

Physical and chemical properties              
Serial Number Test items Units Specifications Measured results Inspection method or instrument
1 Chemical composition Me (wt%) 60.0±2.0 60.27 ICP
2 Ni (wt%) 50.5±2.0 50.52
3 Co (wt%) 6.5±1.0 6.49
4 Mn (wt%) 3.2±1.0 3.26
5 Ni (mol%) / 83.0 
6 Co (mol%) / 11.0 
7 Mn (mol%) / 6.0 
8 Fe (wt%) ≤0.01 0.0008
9 Cu (wt%) ≤0.005 0.0006
10 Na (wt%) ≤0.03 0.0087
11 Ca (wt%) ≤0.02 0.0040
12 Zn (wt%) ≤0.005 0.0005
13

Free potassium

(wt%) ≤0.2 0.1296

Acid burette

14 Physical Properties Particle size distribution D10 (μm) ≥4.0 6.23 Laser particle size analyzer
15 D50 (μm) 10.0~14.0 11.43
16 D90 (μm) ≤28.0 20.03
17 BET (m2/g) 0.2~0.7 0.52  Automatic specific surface and porosity analyzer
18

TD

(g/cm3) ≥2.0 2.41

Tapped density measuring instrument

19 pH / ≤12.5 11.81

pH meter

20 Electrochemical Performance First discharge capacity (mAh/g) ≥190.0 200.3  CR2032
0.1/0.1C(4.3-2.8V)
21 First Time Efficiency (%) ≥90.0 91.5 

 


 

 


Packaging requirements: Inner layer sealed plastic bottle, outer layer aluminum-plastic film sealed.
Storage requirements: Sealed, store in a cool, dry place.
Material requires vacuum sealing for storage.
Material is hygroscopic; humidity must be controlled throughout the sheet preparation process.
Electrolyte used for testing: Ternary electrolyte (KLD-LP04).
Electrode baking conditions: Baking at 85℃ for 4 hours.