Details
The material needs to be vacuum sealed for storage
The electrolyte used during testing is NCM electrolyte (KLD-1230C)
Baking conditions for electrode: Bake at 85 ℃ for 4 hours
Lithium ion battery positive electrode, Ni, Co, Mn NCM material, excellent cycling performance, high gram capacity and first effect

Half battery test



Note: CC constant current charging; CV constant voltage charging; DC constant current discharge