Details
- The materials should be stored under vacuum-sealed conditions.
- The electrolyte used for testing is a lithium titanate electrolyte (KLD-LTO01).
- Electrode drying condition: bake at 85°C for 4 hours prior to testing.
- Packaging requirements: Inner layer sealed in a plastic bottle; outer layer wrapped with aluminum-plastic film.
- Storage requirements: Keep sealed and store in a cool, dry place.
Materials need to be stored in a vacuum seal
The electrolyte used in the test is: lithium titanate electrolyte (KLD-LTO01)
Baking condition: bake at 85 ℃ for 4h
Need R&D Support?
Browse key product categories and connect battery materials with Canrd's R&D services for testing, fabrication, and project support.
Experimental Materials
CategoryCathode, anode, electrolyte, separator, and other materials for battery research.
Shop cathode, anode & electrolyte materials →Lab Equipment
CategoryBattery lab equipment for pilot lines, fixtures, and testing workflows.
Browse battery lab equipment →Electrodes & Cells
CategoryCustom electrodes, dry cells, and battery cell components for R&D validation.
View custom battery electrodes & cells →Sodium Electrolyte
CategorySodium-ion electrolyte options for sodium battery research and validation.
Shop sodium battery electrolytes →R&D Services
ServiceFull-chain battery R&D services from material evaluation to cell fabrication and failure analysis.
Explore Canrd R&D services →Material Evaluation
ServiceCharacterization, electrochemical testing, and compatibility evaluation for battery materials.
Evaluate your battery materials →Electrode Fabrication
ServiceCustom electrode sheets and rolls based on your target chemistry and process needs.
Request electrode fabrication →Cell Fabrication
ServiceDry cells, assembled cells, and custom-format cell builds for R&D validation.
Build custom research cells →Contact
PageAsk Canrd to match products, materials, and services for your project.
Get product and R&D support →