The material needs to be sealed and stored.

The electrolyte used during testing is NCM electrolyte (KLD-1230C).

Baking conditions for electrode: Bake at 85 ℃ for 4 hours.

Lithium ion anode electrode material, pre lithiated silicon oxide, no silicon peak, with the characteristics of high capacity and high first effect

Physical and chemical properties

image.png

Half battery test

2a0a1070ade9e6221b8e07acaf693e3.jpg

CC constant current charging; DC constant current discharge

Note: The material is pre lithiated material