Details
Packaging requirements: Vacuum packaging with aluminum-plastic film, outer layer packaged in plastic bags
Storage requirements: Sealed, stored in a cool and dry place

The material needs to be vacuum sealed for storage
The electrolyte used during testing is lithium manganese iron phosphate electrolyte KLD-LMFP03A
Baking conditions for electrode: Bake at 85 ℃ for 4 hours
Product Advantages:
Contact us for tailored quotes on larger quantities & experience exceptional solutions from our experts.
* The lithium-ion cathode material features an irregular spherical morphology (most particle sizes range from 100–200 nm).
* It has a uniform carbon coating layer with a thickness of 3–5 nm, delivering high first-cycle efficiency and excellent rate performance.

Half battery test:




CC constant current charging; CV constant voltage charging; DC constant current discharge