Details
| Canrd | 10*10cm | 5 sheets/pack | Coating | ||||
| NO. | Electrode Name | Model | Main Material | Active Material Capacity (mAh/g) | Loading | Areal Density (mg/cm²) | Areal Capacity (mAh/cm²) |
| 1 | NCM811 Electrode | SY33 | NCM811 Single Crystal | 188 | 94.50% | 9.20 | 1.63 |
| 2 | NCM811 Electrode | SY34 | — | 188 | 94.50% | 21.50 | 3.82 |
| 3 | NCM622 Electrode | SY25 | NCM622 Single Crystal-B | 168 | 96.70% | 10.00 | 1.62 |
| 4 | NCM622 Electrode | SY24 | — | 168 | 96.70% | 21.60 | 3.51 |
| 5 | NCM523 Electrode | SY15 | NCM523 | 165 | 94.00% | 19.70 | 3.06 |
| 6 | NCM523 Electrode | SY13 | NCM523 | 165 | 94.00% | 10.50 | 1.63 |
| 7 | LCO Electrode | LC02 | High Voltage Lithium Cobalt Oxide-Z-4.45V | 178 | 96.40% | 10.00 | 1.72 |
| 8 | LRM Electrode | FL01 | Lithium-rich Manganese-based-E | 280 | 95.00% | 5.96 | 1.59 |
| 9 | Graphite Electrode | SM02 | Natural Graphite (Standard)-A | 340 | 95.70% | 5.80 | 1.89 |
| 10 | Fast Charging Graphite Electrode | SM04 | Fast Charging Graphite-B | 350 | 96.70% | 5.60 | 1.90 |
| 11 | Silicon Carbon Electrode | SC02 | Silicon Carbon Anode 1800 (Porous Carbon Deposited Silicon) | 420 | 95.00% | 4.80 | 1.92 |
| 12 | NFM Electrode | NT02 | Sodium Nickel Iron Manganese Oxide | 127 | 95.50% | 12.27 | 1.49 |
| 13 | NFM Electrode | NT03 | — | 127 | 95.50% | 8.00 | 0.97 |
| 14 | Hard Carbon Electrode | YT02 | Imported Hard Carbon (5 μm) | 300 | 95.50% | 6.00 | 1.72 |
| 15 | LFP Electrode | LF07 | Lithium Iron Phosphate (High Compaction Density) |
150 | 91.50% | 12.30 | 1.69 |
| 16 | LNMO Electrode | NM01 | High Voltage Lithium Nickel Manganese Oxide-B | 130 | 96.00% | 7.50 | 2.00 |
| 17 | NFPP Electrode | NF01 | Sodium Iron Phosphate Pyrophosphate | 100 | 93.50% | 15.30 | 1.43 |
| 18 | Vanadium Pentoxide Electrode | VO02 | Vanadium Pentoxide | 300 | 80.00% | 5.00 | 1.20 |
| 19 | Manganese Dioxide Electrode | MO02 | Modified Manganese Dioxide (γ-phase) - Long Cycle | 100 | 90.00% | 10.00 | 0.90 |
| 20 | Zinc Negative Electrode | ZA01 | Pure Zinc Powder / Alloy Zinc Powder | / | 70.0%–96.0% | 5.0–15.0 | / |
| 21 | Super capacitor dry process electrode | 6M2302001 | YP50 activated carbon | / | 96.0% | 11.50 | / |
| 22 | Zinc–iodine battery electrode | ZIXX01 | iodine-based active substances | / | / | 20-80 | / |
MOQ for Custom Small Electrode Sheets: 10*10cm/pcs,5cs/pack,1pack
To place an order or request a quotation, please Contact Us.
Because it is a single-sided electrode, there will be a roll-up situation after rolling, so the shipped roller-pressed electrode has controlled and compacted to ensure that the electrode is not rolled;
Rolling can improve the compacting density of the electrode, improve the electronic conductivity of the electrode, and improve the bonding.
| Current collector surface density | 3.5 |
| Current collector thickness (um) | 12 (aluminum foil) |
| Electrode size | 10*10cm |
| Active ingredient ratio | 94.5% |
| Electrode types compatible with full-cell batteries (N/P ratio) | SM02XX(1.15);LT01XX(0.95);SC02XX(1.09) |
| Compacted density (g/cc) | 2.50-3.35 (The density value is not provided for the unrolled electrode, please calculate it yourself) |
| Active Materials | Nickel-cobalt-manganese NCM811 (single crystal) |
| Shelf life | Store for six months (vacuum sealed); use within one month of opening. |
| Recommended electrolyte | KLD-1230C |
| Electrode name | NCM811 electrode sheet |
| Electrode number | SY33XX |
| Active material specific capacity (mAh/g) | 188(3.00-4.30V) |
| Test Conditions Statement | At room temperature (25℃), let stand for 4 hours, charge at a 0.1C rate (constant current) to 4.30V, charge at 4.30V constant voltage to 0.02C, let stand for 3 minutes, discharge at a 0.1C rate (constant current) to 3.00V, and let stand for 3 minutes. |
| Test Conditions | Room temperature 25℃, 0.1/0.1C, 3.00-4.30V |
| Electrode surface capacity (mAh/cm2) | 1.63 |
| Coating surface density(mg/cm2) | 9.20 (tolerance is ±2.0%) |
| Usage recommendations | 1. If the electrode sheet is not rolled, it generally needs to be rolled before punching and baking (the compaction density can be referenced from the minimum value in the "Compaction Density" column of this table); 2. Baking conditions: 85-105℃ for 4 hours (if vacuum baking, it needs to be ventilated twice); 3. The areal density needs to be determined according to the actual weight of each small disc. |
1. The electrode should be rolled before use, and the customer needs to arrange the rolling pressure by himself to purchase the electrode that has not been rolled;
2. The areal density shall be determined according to the actual weighing results;
3. Before putting it in the glove box, the punched electrode needs to be vacuum baked at a temperature of 105 °C for 4 hours;
4. This electrode can be matched with our SM0205, LT0101, SC0101 anode electrode;
5. The density of the coating surface does not include the current collector;
6. Theoretical surface capacity mAh/cm2 = coating surface density mg/cm2 * proportion of active substance * gram capacity mAh/g÷1000;
7. The amount of theoretical active substance (mg) = coating surface density mg/cm2 * proportion of active substance * small disc area cm2;
8. The actual weighing calculates the amount of active substance (mg) = (weight of small disc mg - current collector surface density mg/cm2 * small disc area cm2) * proportion of active substance, and calculates the gram capacity according to the amount of active substance actually weighed. Due to the tolerance of the density of the coating surface, the actual weighing shall prevail.

This product must be tested in accordance with the test methods and electrolytes recommended by Canrd
to achieve the corresponding performance.Since the test method and electrolyte have a great influence on
the performance of the battery, any change in the test method or electrolyte may reduce the performance
of the pole piece; be sure to check this information before purchasing.

SY33 represents design number, XX represents batch number
| Current sales batch | Rolled | Unrolled |
| SY3304 | √ | × |

Perguntas Frequentes
Pesquise ou navegue por perguntas comuns para encontrar respostas rapidamente

Precisa de suporte R&D?
Explore categorias principais de produtos e ligue materiais de bateria aos servicos R&D da Canrd.
Materiais experimentais
CategoriaCatodos, anodos, eletrolitos, separadores e outros materiais para investigacao de baterias.
Comprar materiais de catodo, anodo e eletrolito →Equipamento de laboratorio
CategoriaEquipamento de laboratorio de baterias para linhas piloto, fixtures e fluxos de teste.
Ver equipamento de laboratorio de baterias →Eletrodos e celulas
CategoriaEletrodos personalizados, celulas secas e componentes de celulas para validacao R&D.
Ver eletrodos e celulas de bateria personalizados →Eletrolito de sodio
CategoriaOpcoes de eletrolito de ioes de sodio para investigacao e validacao de baterias de sodio.
Comprar eletrolitos de bateria de sodio →Servicos R&D
ServicoServicos completos de R&D de baterias, da avaliacao de materiais a fabricacao de celulas e analise de falhas.
Explorar servicos R&D da Canrd →Avaliacao de materiais
ServicoCaracterizacao, testes eletroquimicos e avaliacao de compatibilidade para materiais de bateria.
Avaliar os seus materiais de bateria →Fabricacao de eletrodos
ServicoFolhas e rolos de eletrodos personalizados conforme a quimica e processo alvo.
Solicitar fabricacao de eletrodos →Fabricacao de celulas
ServicoCelulas secas, celulas montadas e formatos personalizados para validacao R&D.
Construir celulas de investigacao personalizadas →Contacto
PaginaPeca a Canrd para combinar produtos, materiais e servicos para o seu projeto.
Obter suporte de produto e R&D →