Details
The electrode sheet test requires activation at 0.1C for 5 weeks
| Canrd | 10*10cm | 5 sheets/pack | Coating | ||||
| NO. | Electrode Name | Model | Main Material | Active Material Capacity (mAh/g) | Loading | Areal Density (mg/cm²) | Areal Capacity (mAh/cm²) |
| 1 | NCM811 Electrode | SY33 | NCM811 Single Crystal | 188 | 94.50% | 9.20 | 1.63 |
| 2 | NCM811 Electrode | SY34 | — | 188 | 94.50% | 21.50 | 3.82 |
| 3 | NCM622 Electrode | SY25 | NCM622 Single Crystal-B | 168 | 96.70% | 10.00 | 1.62 |
| 4 | NCM622 Electrode | SY24 | — | 168 | 96.70% | 21.60 | 3.51 |
| 5 | NCM523 Electrode | SY15 | NCM523 | 165 | 94.00% | 19.70 | 3.06 |
| 6 | NCM523 Electrode | SY13 | NCM523 | 165 | 94.00% | 10.50 | 1.63 |
| 7 | LCO Electrode | LC02 | High Voltage Lithium Cobalt Oxide-Z-4.45V | 178 | 96.40% | 10.00 | 1.72 |
| 8 | LRM Electrode | FL01 | Lithium-rich Manganese-based-E | 280 | 95.00% | 5.96 | 1.59 |
| 9 | Graphite Electrode | SM02 | Natural Graphite (Standard)-A | 340 | 95.70% | 5.80 | 1.89 |
| 10 | Fast Charging Graphite Electrode | SM04 | Fast Charging Graphite-B | 350 | 96.70% | 5.60 | 1.90 |
| 11 | Silicon Carbon Electrode | SC02 | Silicon Carbon Anode 1800 (Porous Carbon Deposited Silicon) | 420 | 95.00% | 4.80 | 1.92 |
| 12 | NFM Electrode | NT02 | Sodium Nickel Iron Manganese Oxide | 127 | 95.50% | 12.27 | 1.49 |
| 13 | NFM Electrode | NT03 | — | 127 | 95.50% | 8.00 | 0.97 |
| 14 | Hard Carbon Electrode | YT02 | Imported Hard Carbon (5 μm) | 300 | 95.50% | 6.00 | 1.72 |
| 15 | LFP Electrode | LF07 | Lithium Iron Phosphate (High Compaction Density) |
150 | 91.50% | 12.30 | 1.69 |
| 16 | LNMO Electrode | NM01 | High Voltage Lithium Nickel Manganese Oxide-B | 130 | 96.00% | 7.50 | 2.00 |
| 17 | NFPP Electrode | NF01 | Sodium Iron Phosphate Pyrophosphate | 100 | 93.50% | 15.30 | 1.43 |
| 18 | Vanadium Pentoxide Electrode | VO02 | Vanadium Pentoxide | 300 | 80.00% | 5.00 | 1.20 |
| 19 | Manganese Dioxide Electrode | MO02 | Modified Manganese Dioxide (γ-phase) - Long Cycle | 100 | 90.00% | 10.00 | 0.90 |
| 20 | Zinc Negative Electrode | ZA01 | Pure Zinc Powder / Alloy Zinc Powder | / | 70.0%–96.0% | 5.0–15.0 | / |
| 21 | Super capacitor dry process electrode | 6M2302001 | YP50 activated carbon | / | 96.0% | 11.5 | / |
| 22 | Zinc–iodine battery electrode | ZIXX01 | iodine-based active substances | / | / | 20-80 | / |
MOQ for Custom Small Electrode Sheets: 10*10cm/pcs,5cs/pack,1pack
To place an order or request a quotation, please Contact Us.
Half battery test:




| Current gathering surface density(mg/cm2) | 3.3 |
| Electrode sheet dimensions | 10*10 |
| Current collector thickness(um) | 14(Carbon-coated aluminum foil) |
| Proportion of active substances | 96.00% |
| Compatible electrode sheet models for full batteries (N/P ratio) | nothing |
| Compaction density(g/cc) | 1.80-2.30(The compaction value of the unrolled electrode sheet is not provided. Calculate it by yourself) |
| Active material | High-Voltage Lithium Nickel Manganese Oxide - B |
| Types of current collectors | Carbon-coated aluminum foil |
| Expiration date | It should be stored in vacuum packaging for half a year and used up within one month after opening |
| Recommended electrolyte | KLD-1230C |
| Name of electrode sheet | LNMO High-Voltage Lithium Nickel Manganese Oxide Electrode |
| Electrode plate number | NM01XX |
| Gram capacity of active materials(mAh/g) | 130(3.00-4.95V) |
| Test Condition Description | At room temperature of 25℃, stand for 4 hours, charge at 0.1C rate (constant current) to 4.95V, stand for 3 minutes, discharge at 0.1C rate (constant current) to 3.00V, stand for 3 minutes. |
| Test condition | At 25°C (Room Temperature), 0.1/0.1C, 3.00–4.95 V |
| Areal Capacity(mAh/cm2) | 2 |
| Density of the coating layer(mg/cm2) | 7.50(The tolerance is ±2.0%) |
| Usage Guidelines | "1. If the electrode sheet is not rolled, it is generally necessary to roll it first before punching and baking (the compaction density can be referred to the minimum value in the "Compaction Density" column of this table); 2. Baking conditions: Bake at 85-105℃ for 4 hours (if vacuum baking, air change is required twice); 3. The surface density should be determined based on the actual weighing result of each small disc." |
1. Store under vacuum, or seal with two layers of ziplock bags inside a glove box. This is especially critical for high-nickel cathode materials and sodium-ion battery cathode materials; improper storage will cause an increase in battery internal resistance.
2. The electrodes are uncalendered. Please calender the electrodes in accordance with the recommended compaction density.
3. The coating areal density shall be determined based on actual weighing results, excluding the current collector.
4. Actual active material mass (mg) = (Weight of circular disc (mg) − Areal density of current collector (mg/cm²) × Area of circular disc (cm²)) × Active material content ratio
5. Theoretical active material mass (mg) = Coating areal density (mg/cm²) × Active material content ratio × Area of circular disc (cm²)
6. Theoretical areal capacity (mAh/cm²) = Coating areal density (mg/cm²) × Active material content ratio × Specific capacity (mAh/g) ÷ 1000
7. The specific capacity shall be calculated based on the actual measured mass of active material. Due to tolerance in coating areal density, actual weighing data shall prevail.
8. Creases: Single-sided electrodes tend to curl after calendering. Flattening for packaging may result in creases.
Perguntas Frequentes
Pesquise ou navegue por perguntas comuns para encontrar respostas rapidamente

Precisa de suporte R&D?
Explore categorias principais de produtos e ligue materiais de bateria aos servicos R&D da Canrd.
Materiais experimentais
CategoriaCatodos, anodos, eletrolitos, separadores e outros materiais para investigacao de baterias.
Comprar materiais de catodo, anodo e eletrolito →Equipamento de laboratorio
CategoriaEquipamento de laboratorio de baterias para linhas piloto, fixtures e fluxos de teste.
Ver equipamento de laboratorio de baterias →Eletrodos e celulas
CategoriaEletrodos personalizados, celulas secas e componentes de celulas para validacao R&D.
Ver eletrodos e celulas de bateria personalizados →Eletrolito de sodio
CategoriaOpcoes de eletrolito de ioes de sodio para investigacao e validacao de baterias de sodio.
Comprar eletrolitos de bateria de sodio →Servicos R&D
ServicoServicos completos de R&D de baterias, da avaliacao de materiais a fabricacao de celulas e analise de falhas.
Explorar servicos R&D da Canrd →Avaliacao de materiais
ServicoCaracterizacao, testes eletroquimicos e avaliacao de compatibilidade para materiais de bateria.
Avaliar os seus materiais de bateria →Fabricacao de eletrodos
ServicoFolhas e rolos de eletrodos personalizados conforme a quimica e processo alvo.
Solicitar fabricacao de eletrodos →Fabricacao de celulas
ServicoCelulas secas, celulas montadas e formatos personalizados para validacao R&D.
Construir celulas de investigacao personalizadas →Contacto
PaginaPeca a Canrd para combinar produtos, materiais e servicos para o seu projeto.
Obter suporte de produto e R&D →