Details
1. Due to the small particle size and large specific surface area of the material, compared with the positive electrode formula of ordinary LiCoO2, more conductive and adhesive agents are required to ensure good electronic transmission network.
2. Due to the small particle size, the compaction density of the electrode sheet is 0.3-0.5g/cc lower than that of conventional LiCoO2.
1. MA-EN-CA-0R lithium cobalt oxide, single crystal structure, with small particle size and large specific surface area, facilitating rapid insertion and extraction of lithium ions, resulting in excellent rate performance and good cycling stability.
2. Good processability and stable quality for commercial mass production.
3. Widely used in high-rate requirement products such as drones and electronic cigarettes.
4. Convenient for research on pouch cells and coin cells.
| Test Item | Unit | Specification | Measured Result | Test Method | |
|---|---|---|---|---|---|
| Chemical Composition | Co | (%) | ≥58.5 | 59.82 | ICP |
| Li | (%) | 7.0±0.3 | 7.20 | ||
| Mg | (ppm) | 700~1100 | 923.0 | ||
| Ti | (ppm) | 1300~1700 | 1489.0 | ||
| Al | (ppm) | 200~600 | 325.2 | ||
| Magnetic Substances | (ppb) | ≤300.0 | 27.50 | Acid Titration | |
| Physical Properties | Particle Size Distribution - D10 | (μm) | ≥2.0 | 3.526 | Laser Particle Size Analyzer |
| Particle Size Distribution - D50 | (μm) | 6.4±1.0 | 6.728 | ||
| Particle Size Distribution - D90 | (μm) | ≤20.0 | 10.920 | ||
| BET | (m2/g) | 0.3~0.6 | 0.40 | Automated Surface Area & Porosity | |
| TD | (g/cm3) | ≥2.0 | 2.38 | Tap Density Tester | |
| pH | / | ≤11.2 | 10.52 | pH Meter | |
| Moisture | (ppm) | ≤300 | 128.2 | Moisture Analyzer | |
| Electrochemical Performance | Initial Discharge Capacity | (mAh/g) | ≥170.0 | 175.9 | CR2032 |
| Initial Efficiency | (%) | ≥97.0 | 98.4 | 0.1/0.1C(4.40-3.00V) | |
SEM image:

Charge/discharge curve:




1. Storage conditions: sealed storage at room temperature.
2. Shelf life: 2 years from the production date.
Remarks:
1、CC – Constant Current Charge; DC – Constant Current Discharge; CV – Constant Voltage Charge
2、Recommended Electrolyte: Lithium Cobalt Oxide Electrolyte (KLD-1376)
Precisa de suporte R&D?
Explore categorias principais de produtos e ligue materiais de bateria aos servicos R&D da Canrd.
Materiais experimentais
CategoriaCatodos, anodos, eletrolitos, separadores e outros materiais para investigacao de baterias.
Comprar materiais de catodo, anodo e eletrolito →Equipamento de laboratorio
CategoriaEquipamento de laboratorio de baterias para linhas piloto, fixtures e fluxos de teste.
Ver equipamento de laboratorio de baterias →Eletrodos e celulas
CategoriaEletrodos personalizados, celulas secas e componentes de celulas para validacao R&D.
Ver eletrodos e celulas de bateria personalizados →Eletrolito de sodio
CategoriaOpcoes de eletrolito de ioes de sodio para investigacao e validacao de baterias de sodio.
Comprar eletrolitos de bateria de sodio →Servicos R&D
ServicoServicos completos de R&D de baterias, da avaliacao de materiais a fabricacao de celulas e analise de falhas.
Explorar servicos R&D da Canrd →Avaliacao de materiais
ServicoCaracterizacao, testes eletroquimicos e avaliacao de compatibilidade para materiais de bateria.
Avaliar os seus materiais de bateria →Fabricacao de eletrodos
ServicoFolhas e rolos de eletrodos personalizados conforme a quimica e processo alvo.
Solicitar fabricacao de eletrodos →Fabricacao de celulas
ServicoCelulas secas, celulas montadas e formatos personalizados para validacao R&D.
Construir celulas de investigacao personalizadas →Contacto
PaginaPeca a Canrd para combinar produtos, materiais e servicos para o seu projeto.
Obter suporte de produto e R&D →