Details
The material needs to be vacuum sealed for storage
The material is prone to water absorption, and humidity control is required throughout the entire production process
The electrolyte used during testing is NCM electrolyte (KLD-1230C)
Baking conditions for electrode: Bake at 85 ℃ for 4 hours
Lithium ion battery cathode electrode, Ni, Co, Mn NCM material, morphology as secondary sphere, excellent rate performance
Physical and chemical properties

Half battery test:




CC rate charging, CV constant voltage charging, DC rate discharging