NiCobalt-Manganese NCM613 (Polycrystalline)
NiCobalt-Manganese NCM613 (Polycrystalline)
NiCobalt-Manganese NCM613 (Polycrystalline)
NiCobalt-Manganese NCM613 (Polycrystalline)
NiCobalt-Manganese NCM613 (Polycrystalline)

NiCobalt-Manganese NCM613 (Polycrystalline)

$39.26
Model:
MA-EN-CA-0047
item_No
Specifications
Price
MA-EN-CA-004701
20g
$39.26

Details

Lithium ion battery cathode electrode, Ni, Co, Mn NCM material, morphology as secondary sphere, excellent rate performance

Physical and chemical properties

Test Category Test Item Unit Specification Measured Result Test Method or Instrument
Chemical Composition Li wt% 7.0±2.0 7.52 ICP
Co+Ni+Mn wt% 60.0±3.0 58.88 ICP
Ca wt% ≤0.01 0.0015 ICP
Fe wt% ≤0.01 0.0014 ICP
Mg wt% ≤0.01 0.0015 ICP
Na wt% ≤0.01 0.0095 ICP
Free Lithium wt% ≤0.5 0.0774 Acid burette
Physical Properties Particle Size Distribution: D10 μm ≥1.0 2.330 Laser Particle Size Analyzer
Particle Size Distribution: D50 μm 4.0~6.0 5.058 Laser Particle Size Analyzer
Particle Size Distribution: D90 μm ≤15.0 10.881 Laser Particle Size Analyzer
BET m²/g ≥0.5 0.78 Automatic Specific Surface & Porosity Analyzer
TD (Tap Density) g/cm³ ≤3.0 1.95 Tap Density Tester
Moisture Content ppm ≤600 166.3 Moisture Analyzer
Electrochemical Performance Initial Discharge Capacity mAh/g ≥165.0 175.1 CR2032 coin cell, 0.1/0.1C (4.3-2.8V)
Initial Coulombic Efficiency % ≥87.0 88.2 CR2032 coin cell, 0.1/0.1C (4.3-2.8V)

Half battery test

 

CC rate charging, CV constant voltage charging, DC rate discharging

 

Packaging Requirements: Inner plastic bottle sealed; outer layer enclosed in aluminum-plastic film.Storage Requirements: Store in a sealed container, isolated from strong oxidizers. Strictly prohibit storage in humid or high-temperature environments.
Shelf Life: 1 year from the date of manufacture.

The materials must be stored under vacuum-sealed conditions.
As the materials are highly hygroscopic, humidity must be strictly controlled throughout the entire electrode fabrication process.
The electrolyte used for testing is a ternary electrolyte (KLD-1230C).
Electrode drying conditions: 85°C for 4 hours.