Details
1. Due to the small particle size and large specific surface area of the material, compared with the positive electrode formula of ordinary LiCoO2, more conductive and adhesive agents are required to ensure good electronic transmission network.
2. Due to the small particle size, the compaction density of the electrode sheet is 0.3-0.5g/cc lower than that of conventional LiCoO2.
1. MA-EN-CA-0R lithium cobalt oxide, single crystal structure, with small particle size and large specific surface area, facilitating rapid insertion and extraction of lithium ions, resulting in excellent rate performance and good cycling stability.
2. Good processability and stable quality for commercial mass production.
3. Widely used in high-rate requirement products such as drones and electronic cigarettes.
4. Convenient for research on pouch cells and coin cells.
| Test Item | Unit | Specification | Measured Result | Test Method | |
|---|---|---|---|---|---|
| Chemical Composition | Co | (%) | ≥58.5 | 59.82 | ICP |
| Li | (%) | 7.0±0.3 | 7.20 | ||
| Mg | (ppm) | 700~1100 | 923.0 | ||
| Ti | (ppm) | 1300~1700 | 1489.0 | ||
| Al | (ppm) | 200~600 | 325.2 | ||
| Magnetic Substances | (ppb) | ≤300.0 | 27.50 | Acid Titration | |
| Physical Properties | Particle Size Distribution - D10 | (μm) | ≥2.0 | 3.526 | Laser Particle Size Analyzer |
| Particle Size Distribution - D50 | (μm) | 6.4±1.0 | 6.728 | ||
| Particle Size Distribution - D90 | (μm) | ≤20.0 | 10.920 | ||
| BET | (m2/g) | 0.3~0.6 | 0.40 | Automated Surface Area & Porosity | |
| TD | (g/cm3) | ≥2.0 | 2.38 | Tap Density Tester | |
| pH | / | ≤11.2 | 10.52 | pH Meter | |
| Moisture | (ppm) | ≤300 | 128.2 | Moisture Analyzer | |
| Electrochemical Performance | Initial Discharge Capacity | (mAh/g) | ≥170.0 | 175.9 | CR2032 |
| Initial Efficiency | (%) | ≥97.0 | 98.4 | 0.1/0.1C(4.40-3.00V) | |
SEM image:

Charge/discharge curve:




1. Storage conditions: sealed storage at room temperature.
2. Shelf life: 2 years from the production date.
Remarks:
1、CC – Constant Current Charge; DC – Constant Current Discharge; CV – Constant Voltage Charge
2、Recommended Electrolyte: Lithium Cobalt Oxide Electrolyte (KLD-1376)
Necesitas soporte R&D?
Explora categorias clave de productos y conecta materiales de bateria con los servicios R&D de Canrd.
Materiales experimentales
CategoriaCatodos, anodos, electrolitos, separadores y otros materiales para investigacion de baterias.
Comprar materiales de catodo, anodo y electrolito →Equipos de laboratorio
CategoriaEquipos de laboratorio de baterias para lineas piloto, utillajes y flujos de prueba.
Ver equipos de laboratorio de baterias →Electrodos y celdas
CategoriaElectrodos personalizados, celdas secas y componentes de celdas para validacion R&D.
Ver electrodos y celdas de bateria personalizados →Electrolito de sodio
CategoriaOpciones de electrolito de ion sodio para investigacion y validacion de baterias de sodio.
Comprar electrolitos de bateria de sodio →Servicios R&D
ServicioServicios completos de R&D de baterias, desde evaluacion de materiales hasta fabricacion de celdas y analisis de fallos.
Explorar servicios R&D de Canrd →Evaluacion de materiales
ServicioCaracterizacion, pruebas electroquimicas y evaluacion de compatibilidad para materiales de bateria.
Evaluar tus materiales de bateria →Fabricacion de electrodos
ServicioLaminas y rollos de electrodos personalizados segun tu quimica y proceso objetivo.
Solicitar fabricacion de electrodos →Fabricacion de celdas
ServicioCeldas secas, celdas ensambladas y formatos personalizados para validacion R&D.
Construir celdas de investigacion personalizadas →Contacto
PaginaPide a Canrd combinar productos, materiales y servicios para tu proyecto.
Obtener soporte de producto y R&D →