Details
1.Materials need to be vacuum sealed for storage
2.The material is easy to absorb water, and humidity needs to be controlled throughout the production process
3.The electrolyte used during testing is: NCM electrolyte (KLD-1230C)
4.Baking conditions for electrodes: bake at 85 ℃ for 4 hours
Lithium ion cathode electrode, ternary high nickel Ni, Co, Al material, polycrystalline structure, spherical shape, with the characteristic of high gram capacity
Physical and chemical properties

Half battery test:




CC rate charging; CV constant voltage charging; DC rate discharge