Details
This NCM811 electrode sheet (SY34XX) is developed for advanced lithium-ion battery research, featuring a single-crystal nickel-cobalt-manganese (NCM811) active material with a high active material ratio of 94.5%. The electrode, coated on a 12 µm aluminum foil current collector, delivers a specific capacity of 188 mAh/g (3.00–4.30V) and an areal capacity of 3.82 mAh/cm², with a coating areal density of 21.50 mg/cm². Available in both roll-pressed and unrolled configurations, the unrolled sheets require custom compaction. Designed for full-cell testing with the recommended electrolyte KLD-1230C, this electrode supports a 6-month shelf life under vacuum sealing and is typically used in laboratory-scale coin cells or small pouch cells. Its high nickel content and single-crystal structure make it suitable for studying high-energy-density cathode performance.
| Canrd | 10*10cm | 5 sheets/pack | Coating | ||||
| NO. | Electrode Name | Model | Main Material | Active Material Capacity (mAh/g) | Loading | Areal Density (mg/cm²) | Areal Capacity (mAh/cm²) |
| 1 | NCM811 Electrode | SY33 | NCM811 Single Crystal | 188 | 94.50% | 9.20 | 1.63 |
| 2 | NCM811 Electrode | SY34 | — | 188 | 94.50% | 21.50 | 3.82 |
| 3 | NCM622 Electrode | SY25 | NCM622 Single Crystal-B | 168 | 96.70% | 10.00 | 1.62 |
| 4 | NCM622 Electrode | SY24 | — | 168 | 96.70% | 21.60 | 3.51 |
| 5 | NCM523 Electrode | SY15 | NCM523 | 165 | 94.00% | 19.70 | 3.06 |
| 6 | NCM523 Electrode | SY13 | NCM523 | 165 | 94.00% | 10.50 | 1.63 |
| 7 | LCO Electrode | LC02 | High Voltage Lithium Cobalt Oxide-Z-4.45V | 178 | 96.40% | 10.00 | 1.72 |
| 8 | LRM Electrode | FL01 | Lithium-rich Manganese-based-E | 280 | 95.00% | 5.96 | 1.59 |
| 9 | Graphite Electrode | SM02 | Natural Graphite (Standard)-A | 340 | 95.70% | 5.80 | 1.89 |
| 10 | Fast Charging Graphite Electrode | SM04 | Fast Charging Graphite-B | 350 | 96.70% | 5.60 | 1.90 |
| 11 | Silicon Carbon Electrode | SC02 | Silicon Carbon Anode 1800 (Porous Carbon Deposited Silicon) | 420 | 95.00% | 4.80 | 1.92 |
| 12 | NFM Electrode | NT02 | Sodium Nickel Iron Manganese Oxide | 127 | 95.50% | 12.27 | 1.49 |
| 13 | NFM Electrode | NT03 | — | 127 | 95.50% | 8.00 | 0.97 |
| 14 | Hard Carbon Electrode | YT02 | Imported Hard Carbon (5 μm) | 300 | 95.50% | 6.00 | 1.72 |
| 15 | LFP Electrode | LF07 | Lithium Iron Phosphate (High Compaction Density) |
150 | 91.50% | 12.30 | 1.69 |
| 16 | LNMO Electrode | NM01 | High Voltage Lithium Nickel Manganese Oxide-B | 130 | 96.00% | 7.50 | 2.00 |
| 17 | NFPP Electrode | NF01 | Sodium Iron Phosphate Pyrophosphate | 100 | 93.50% | 15.30 | 1.43 |
| 18 | Vanadium Pentoxide Electrode | VO02 | Vanadium Pentoxide | 300 | 80.00% | 5.00 | 1.20 |
| 19 | Manganese Dioxide Electrode | MO02 | Modified Manganese Dioxide (γ-phase) - Long Cycle | 100 | 90.00% | 10.00 | 0.90 |
| 20 | Zinc Negative Electrode | ZA01 | Pure Zinc Powder / Alloy Zinc Powder | / | 70.0%–96.0% | 5.0–15.0 | / |
| 21 | Super capacitor dry process electrode | 6M2302001 | YP50 activated carbon | / | 96.0% | 11.50 | / |
| 22 | Zinc–iodine battery electrode | ZIXX01 | iodine-based active substances | / | / | 20-80 | / |
MOQ for Custom Small Electrode Sheets: 10*10cm/pcs,5cs/pack,1pack
To place an order or request a quotation, please Contact Us.


| Current collector areal density (mg/cm²) | 3.40 |
| Electrode size | 10*10 |
| Current collector thickness (µm) | 12 (Aluminum foil) |
| Active material ratio | 94.5% |
| Compatible electrode type for full cells (N/P ratio) | None (Customization is available upon request). |
| Pack density (g/cc) | 2.50-3.35 (Compaction value not provided for unrolled electrode sheets; calculate it yourself) |
| Active material | Nickel-Cobalt-Manganese NCM811 (Single Crystal) |
| Shelf life | 6 months (vacuum sealed). Use within one month of opening. |
| Recommended electrolyte | KLD-1230C |
| Electrode name | NCM811 electrode sheet |
| Electrode number | SY34XX |
| Active material specific capacity (mAh/g) | 188(3.00-4.30V) |
| Test conditions description | At room temperature (25℃), let stand for 4 hours, charge at a 0.1C rate (constant current) to 4.30V, charge at 4.30V constant voltage to 0.02C, let stand for 3 minutes, discharge at a 0.1C rate (constant current) to 3.00V, and let stand for 3 minutes. |
| Test condition | At room temperature (25℃), 0.1/0.1C, 3.00-4.30V |
| Areal capacity (mAh/cm²) | 3.82 |
| Coating areal density (mg/cm²) | 21.50 (tolerance ±2.0%) |
| Usage recommendations |
1. If the electrode sheet is not rolled, it generally needs to be rolled before punching and baking (the compaction density can be referenced from the minimum value in the "Compaction Density" column of this table); 2. Baking conditions: 85-105℃ for 4 hours (if vacuum baking, two air changes are required); |
Häufig gestellte Fragen
Durchsuchen oder durchstöbern Sie häufige Fragen, um schnell Antworten zu finden

Benötigen Sie R&D-Unterstützung?
Entdecken Sie wichtige Produktkategorien und verbinden Sie Batteriematerialien mit Canrds R&D-Services.
Experimentelle Materialien
KategorieKathoden, Anoden, Elektrolyte, Separatoren und weitere Materialien für Batterieforschung.
Kathoden-, Anoden- und Elektrolytmaterialien kaufen →Laborgeräte
KategorieBatterielaborgeräte für Pilotlinien, Vorrichtungen und Testabläufe.
Batterielaborgeräte ansehen →Elektroden und Zellen
KategorieKundenspezifische Elektroden, Trockenzellen und Zellkomponenten für R&D-Validierung.
Kundenspezifische Batterieelektroden und Zellen ansehen →Natrium-Elektrolyt
KategorieNatrium-Ionen-Elektrolyte für Natriumbatterieforschung und Validierung.
Natrium-Batterieelektrolyte kaufen →R&D-Services
ServiceGanzheitliche Batterie-R&D-Services von Materialbewertung bis Zellfertigung und Fehleranalyse.
Canrd R&D-Services entdecken →Materialbewertung
ServiceCharakterisierung, elektrochemische Tests und Kompatibilitätsbewertung für Batteriematerialien.
Batteriematerialien bewerten lassen →Elektrodenfertigung
ServiceKundenspezifische Elektrodenblätter und -rollen für Ihre Zielchemie und Prozessanforderungen.
Elektrodenfertigung anfragen →Zellfertigung
ServiceTrockenzellen, montierte Zellen und kundenspezifische Zellformate für R&D-Validierung.
Kundenspezifische Forschungszellen bauen →Kontakt
SeiteCanrd kann Produkte, Materialien und Services passend zu Ihrem Projekt kombinieren.
Produkt- und R&D-Support erhalten →