Details
The material needs to be vacuum sealed for storage
The electrolyte used during testing is silicon carbon electrolyte (KLD-Si01)
Baking conditions for polarizer: Bake at 85 ℃ for 4 hours
Lithium ion anode electrode material, porous carbon skeleton

Half battery test:

SEM