Details
| Canrd | 10*10cm | 5 sheets/pack | Coating | ||||
| NO. | Electrode Name | Model | Main Material | Active Material Capacity (mAh/g) | Loading | Areal Density (mg/cm²) | Areal Capacity (mAh/cm²) |
| 1 | NCM811 Electrode | SY33 | NCM811 Single Crystal | 188 | 94.50% | 9.20 | 1.63 |
| 2 | NCM811 Electrode | SY34 | — | 188 | 94.50% | 21.50 | 3.82 |
| 3 | NCM622 Electrode | SY25 | NCM622 Single Crystal-B | 168 | 96.70% | 10.00 | 1.62 |
| 4 | NCM622 Electrode | SY24 | — | 168 | 96.70% | 21.60 | 3.51 |
| 5 | NCM523 Electrode | SY15 | NCM523 | 165 | 94.00% | 19.70 | 3.06 |
| 6 | NCM523 Electrode | SY13 | NCM523 | 165 | 94.00% | 10.50 | 1.63 |
| 7 | LCO Electrode | LC02 | High Voltage Lithium Cobalt Oxide-Z-4.45V | 178 | 96.40% | 10.00 | 1.72 |
| 8 | LRM Electrode | FL01 | Lithium-rich Manganese-based-E | 280 | 95.00% | 5.96 | 1.59 |
| 9 | Graphite Electrode | SM02 | Natural Graphite (Standard)-A | 340 | 95.70% | 5.80 | 1.89 |
| 10 | Fast Charging Graphite Electrode | SM04 | Fast Charging Graphite-B | 350 | 96.70% | 5.60 | 1.90 |
| 11 | Silicon Carbon Electrode | SC02 | Silicon Carbon Anode 1800 (Porous Carbon Deposited Silicon) | 420 | 95.00% | 4.80 | 1.92 |
| 12 | NFM Electrode | NT02 | Sodium Nickel Iron Manganese Oxide | 127 | 95.50% | 12.27 | 1.49 |
| 13 | NFM Electrode | NT03 | — | 127 | 95.50% | 8.00 | 0.97 |
| 14 | Hard Carbon Electrode | YT02 | Imported Hard Carbon (5 μm) | 300 | 95.50% | 6.00 | 1.72 |
| 15 | LFP Electrode | LF07 | Lithium Iron Phosphate (High Compaction Density) |
150 | 91.50% | 12.30 | 1.69 |
| 16 | LNMO Electrode | NM01 | High Voltage Lithium Nickel Manganese Oxide-B | 130 | 96.00% | 7.50 | 2.00 |
| 17 | NFPP Electrode | NF01 | Sodium Iron Phosphate Pyrophosphate | 100 | 93.50% | 15.30 | 1.43 |
| 18 | Vanadium Pentoxide Electrode | VO02 | Vanadium Pentoxide | 300 | 80.00% | 5.00 | 1.20 |
| 19 | Manganese Dioxide Electrode | MO02 | Modified Manganese Dioxide (γ-phase) - Long Cycle | 100 | 90.00% | 10.00 | 0.90 |
| 20 | Zinc Negative Electrode | ZA01 | Pure Zinc Powder / Alloy Zinc Powder | / | 70.0%–96.0% | 5.0–15.0 | / |
| 21 | Super capacitor dry process electrode | 6M2302001 | YP50 activated carbon | / | 96.0% | 11.50 | / |
| 22 | Zinc–iodine battery electrode | ZIXX01 | iodine-based active substances | / | / | 20-80 | / |
MOQ for Custom Small Electrode Sheets: 10*10cm/pcs,5cs/pack,1pack
To place an order or request a quotation, please Contact Us.
Rolling can increase the compaction density of the electrode, improve the electronic conductivity of the electrode, and enhance adhesion
1. The surface density needs to be determined based on the actual weighing results
2. Before placing it in the glove box, the punched polarizer needs to be vacuum baked at 105 ℃ for 4 hours
3. The surface density of the coating does not include the current collector;
4. Theoretical surface capacity mAh/cm2=coating surface density mg/cm2 * active material ratio * gram capacity mAh/g ÷ 1000
5. Theoretical amount of active substance (mg)=coating surface density mg/cm2 * active substance ratio * small disc area cm2
6. The actual amount of active substance calculated by weighing (mg)=(weight of small disc mg - current collector surface density mg/cm2 * area of small disc cm2) * proportion of active substance
7. When calculating the gram capacity, the actual amount of active substance weighed shall be used. Due to the tolerance of the coating surface density, the actual weight shall prevail
8. This pole piece can be matched with our SM02XX, LT01XX, SC01XX negative pole pieces for use
This product must be tested in accordance with the test methods and electrolytes recommended by
Canrd to achieve the corresponding performance.Since the test method and electrolyte have a great
influence on the performance of the battery, any change in the test method or electrolyte may reduce
the performance of the pole piece; be sure to check this information before purchasing.
Customized (5 Pcs / Pack): Please Quote.



First charge and discharge test conditions: temperature 25 ℃, first charge at a constant current of 0.1C to 4.3V, then charge at a constant voltage until the current is less than 0.02C, and then discharge at a constant current of 0.1C to 3.0V
Rate test conditions: Temperature of 25 ℃, first charge at a constant current of 0.5C to 4.3V, then charge at a constant voltage until the current is less than 0.02C, and then discharge at a constant current rate of 0.1C/0.2C/0.5C/1C/2C/3C to 3.0V
Cycle test conditions: temperature 25 ℃, first charge at 0.5C constant current to 4.3V, then charge at constant voltage until the current is less than 0.02C, and then discharge at 1C constant current to 3.0V
الأسئلة الشائعة
ابحث أو تصفح الأسئلة الشائعة للعثور على الإجابات بسرعة

هل تحتاج إلى دعم البحث والتطوير؟
تصفح فئات المنتجات الرئيسية واربط مواد البطاريات بخدمات البحث والتطوير من Canrd.
مواد تجريبية
فئةكاثودات وأنودات وإلكتروليتات وفواصل ومواد أخرى لأبحاث البطاريات.
تصفح مواد الكاثود والأنود والإلكتروليت →معدات المختبر
فئةمعدات مختبر البطاريات لخطوط التجربة والتركيبات وسير عمل الاختبار.
تصفح معدات مختبر البطاريات →الأقطاب والخلايا
فئةأقطاب مخصصة وخلايا جافة ومكونات خلايا بطارية للتحقق في البحث والتطوير.
عرض أقطاب وخلايا البطاريات المخصصة →إلكتروليت الصوديوم
فئةخيارات إلكتروليت أيون الصوديوم لأبحاث بطاريات الصوديوم والتحقق منها.
تصفح إلكتروليتات بطاريات الصوديوم →خدمات البحث والتطوير
خدمةخدمات بحث وتطوير كاملة من تقييم المواد إلى تصنيع الخلايا وتحليل الأعطال.
استكشف خدمات البحث والتطوير من Canrd →تقييم المواد
خدمةتوصيف واختبارات كهروكيميائية وتقييم توافق لمواد البطاريات.
قيّم مواد البطارية لديك →تصنيع الأقطاب
خدمةصفائح ولفائف أقطاب مخصصة حسب الكيمياء المستهدفة واحتياجات العملية.
اطلب تصنيع الأقطاب →تصنيع الخلايا
خدمةخلايا جافة وخلايا مجمعة وتنسيقات مخصصة للتحقق في البحث والتطوير.
اصنع خلايا بحثية مخصصة →اتصل بنا
صفحةاطلب من Canrd مطابقة المنتجات والمواد والخدمات مع مشروعك.
احصل على دعم المنتج والبحث والتطوير →