Nickel cobalt manganese lithium Ni90 single crystal
Nickel cobalt manganese lithium Ni90 single crystal
Nickel cobalt manganese lithium Ni90 single crystal

Nickel cobalt manganese lithium Ni90 single crystal

$45.31
Molecularformula:
LiNi0.90Co0.05Mn0.05O2
Model:
MA-EN-CA-0002
Classification:
item_No
Specifications
Price
MA-EN-CA-000201
20g
$45.31

Details

This product is a high-nickel single-crystal NCM (Ni90) cathode material developed for advanced lithium-ion battery research. Its single-crystal structure enhances structural stability and delivers high gram capacity, supporting high-energy-density electrode design. The material is moisture-sensitive and requires vacuum sealing with aluminum-plastic film and storage in a cool, dry environment. Electrochemical testing typically uses NCM-specific electrolyte (KLD-1230C) with electrode baking at 85°C for 4 hours. This Ni90 material is commonly applied in half-cell evaluations and studies targeting improved cycling performance and thermal stability for next-generation cathodes.

Lithium ion battery cathode electrode, Ni, Co, Mn NCM material, high nickel, single crystal structure, high gram capacity.

Physical and chemical properties

image.png

Half battery test

02859e541476b63206374575a0e7c84.jpg

83dd0c41ab750cb39c040e1954c6699.jpg

ace70e524d6711d081cf680d0ba411e.jpg

47f5275a3ef5bf67c3282fb1de57de9.jpg

CC rate charging, CV constant voltage charging, DC rate discharging

 

Packaging requirements: Sealed with vacuum aluminum-plastic film, outer layer packed in plastic bags.

Storage requirements: Sealed, stored in a cool and dry place.

 

The material needs to be vacuum sealed for storage.

The material is prone to water absorption, and humidity control is required throughout the entire production process.

The electrolyte used during testing is NCM electrolyte (KLD-1230C).

Baking conditions for electrode: Bake at 85 ℃ for 4 hours.