| Canrd | 10*10cm | 5 sheets/pack | Coating | ||||
| NO. | Electrode Name | Model | Main Material | Active Material Capacity (mAh/g) | Loading | Areal Density (mg/cm²) | Areal Capacity (mAh/cm²) |
| 1 | NCA Electrode | SY51 | NCA-S (Nickel Cobalt Aluminum Oxide) | 195 | 94.50% | 17.66 | 3.25 |
| 2 | Ni90 Electrode | SY41 | Ni90 Single Crystal NCM | 195 | 94.50% | 9.50 | 1.75 |
| 3 | NCM811 Electrode | SY33 | NCM811 Single Crystal | 188 | 94.50% | 9.20 | 1.63 |
| 4 | NCM811 Electrode | SY34 | — | 188 | 94.50% | 21.50 | 3.82 |
| 5 | NCM622 Electrode | SY25 | NCM622 Single Crystal-B | 168 | 96.70% | 10.00 | 1.62 |
| 6 | NCM622 Electrode | SY24 | — | 168 | 96.70% | 21.60 | 3.51 |
| 7 | NCM523 Electrode | SY15 | NCM523 | 165 | 94.00% | 19.70 | 3.06 |
| 8 | NCM523 Electrode | SY13 | NCM523 | 165 | 94.00% | 10.50 | 1.63 |
| 9 | LCO Electrode | LC02 | High Voltage Lithium Cobalt Oxide-Z-4.45V | 178 | 96.40% | 10.00 | 1.72 |
| 10 | LRM Electrode | FL01 | Lithium-rich Manganese-based-E | 280 | 95.00% | 5.96 | 1.59 |
| 11 | Graphite Electrode | SM02 | Natural Graphite (Standard)-A | 340 | 95.70% | 5.80 | 1.89 |
| 12 | Fast Charging Graphite Electrode | SM04 | Fast Charging Graphite-B | 350 | 96.70% | 5.60 | 1.90 |
| 13 | Silicon Carbon Electrode | SC02 | Silicon Carbon Anode 1800 (Porous Carbon Deposited Silicon) | 420 | 95.00% | 4.80 | 1.92 |
| 14 | NFM Electrode | NT02 | Sodium Nickel Iron Manganese Oxide | 127 | 95.50% | 12.27 | 1.49 |
| 15 | NFM Electrode | NT03 | — | 127 | 95.50% | 8.00 | 0.97 |
| 16 | Hard Carbon Electrode | YT02 | Imported Hard Carbon (5 μm) | 300 | 95.50% | 6.00 | 1.72 |
| 17 | LFP Electrode | LF07 | Lithium Iron Phosphate (High Compaction Density) |
150 | 91.50% | 12.30 | 1.69 |
| 18 | LNMO Electrode | NM01 | High Voltage Lithium Nickel Manganese Oxide-B | 130 | 96.00% | 7.50 | 2.00 |
| 19 | NFPP Electrode | NF01 | Sodium Iron Phosphate Pyrophosphate | 100 | 93.50% | 15.30 | 1.43 |
| 20 | Vanadium Pentoxide Electrode | VO02 | Vanadium Pentoxide | 300 | 80.00% | 5.00 | 1.20 |
| 21 | Manganese Dioxide Electrode | MO01 | Manganese-based or Vanadium-based Material | 100 | 80.00% | 5.00 | / |
| 22 | Zinc Negative Electrode | ZA01 | Pure Zinc Powder / Alloy Zinc Powder | / | 70.0%–96.0% | 5.0–15.0 | / |
MOQ for Custom Small Electrode Sheets: 10*10cm/pcs,5cs/pack,1pack
To place an order or request a quotation, please Contact Us.

This product must be tested according to Canrd recommended testing methods and electrolytes to achieve the desired performance.
Because testing methods and electrolytes significantly impact battery performance, changing the testing method or electrolyte may degrade electrode performance. Please verify this information before purchasing.
Electrode Sheet Technical Data Sheet (SC02XX - Si/C 420 Electrode)
| Parameter | Specification |
|---|---|
| Slurry Areal Density (mg/cm²) | 7.25 |
| Electrode Sheet Size | 10 × 10 cm |
| Current Collector Thickness (μm) | 9 (Carbon-coated Cu foil) |
| Active Material Ratio | 95.00% |
| Compacted Density (g/cc) | 1.10 (Not compacted; value needs self-calculation) |
| Active Material | Si/C 1800 (5%) + Graphite (95%) |
| Recommended Electrolyte | KLD-Si01 |
| Electrode Name | Si/C 420 Electrode |
| Electrode Code | SC02XX |
| Specific Capacity (mAh/g) | 420 (0.005–2.000 V) |
| Areal Capacity (mAh/cm²) | 1.9 |
| Coating Areal Density (mg/cm²) | 4.80 (Tolerance ±2.0%) |
Usage Recommendations
-
If the electrode is not compacted, it should be compacted before punching and baking. (Reference minimum value above for compacted density.)
-
Baking conditions: 85–105°C for 4 hours.
If vacuum baking, replace the air twice. -
Active material mass should be weighed for each circular electrode individually for accurate calculation.
Compatible Full Cell Electrode Models (N/P Ratio ≈ 1.09)
SY13XX, SY25XX, SY33XX, LF06XX, LC02XX
Test Conditions
-
Ambient temperature: 25°C, rest for 4 h
-
Discharge: 0.10C / 0.09C / 0.08C / ... / 0.01C (constant current) to 0.005 V
-
Rest for 3 min
-
Charge: 0.1C (constant current) to 2.00 V
-
Rest for 3 min
Shelf Life
-
6 months in vacuum-sealed storage
-
Use within 1 month after opening
Capacity Measurement Conditions
-
25°C
-
0.10 / 0.09 / 0.08 / 0.07 / 0.06 / 0.05 / 0.04 / 0.03 / 0.02 / 0.01 C DC discharge to 0.005 V
-
0.1 C CC charge to 2.00 V
This product must be tested according to Canrd recommended testing methods and electrolytes to achieve the desired performance.
Because testing methods and electrolytes significantly impact battery performance, changing the testing method or electrolyte may degrade electrode performance. Please verify this information before purchasing.
Electrode Sheet Technical Data Sheet (SC02XX - Si/C 420 Electrode)
| Parameter | Specification |
|---|---|
| Slurry Areal Density (mg/cm²) | 7.25 |
| Electrode Sheet Size | 10 × 10 cm |
| Current Collector Thickness (μm) | 9 (Carbon-coated Cu foil) |
| Active Material Ratio | 95.00% |
| Compacted Density (g/cc) | 1.10 (Not compacted; value needs self-calculation) |
| Active Material | Si/C 1800 (5%) + Graphite (95%) |
| Recommended Electrolyte | KLD-Si01 |
| Electrode Name | Si/C 420 Electrode |
| Electrode Code | SC02XX |
| Specific Capacity (mAh/g) | 420 (0.005–2.000 V) |
| Areal Capacity (mAh/cm²) | 1.9 |
| Coating Areal Density (mg/cm²) | 4.80 (Tolerance ±2.0%) |
Usage Recommendations
-
If the electrode is not compacted, it should be compacted before punching and baking. (Reference minimum value above for compacted density.)
-
Baking conditions: 85–105°C for 4 hours.
If vacuum baking, replace the air twice. -
Active material mass should be weighed for each circular electrode individually for accurate calculation.
Compatible Full Cell Electrode Models (N/P Ratio ≈ 1.09)
SY13XX, SY25XX, SY33XX, LF06XX, LC02XX
Test Conditions
-
Ambient temperature: 25°C, rest for 4 h
-
Discharge: 0.10C / 0.09C / 0.08C / ... / 0.01C (constant current) to 0.005 V
-
Rest for 3 min
-
Charge: 0.1C (constant current) to 2.00 V
-
Rest for 3 min
Shelf Life
-
6 months in vacuum-sealed storage
-
Use within 1 month after opening
Capacity Measurement Conditions
-
25°C
-
0.10 / 0.09 / 0.08 / 0.07 / 0.06 / 0.05 / 0.04 / 0.03 / 0.02 / 0.01 C DC discharge to 0.005 V
-
0.1 C CC charge to 2.00 V
This product must be tested according to Canrd recommended testing methods and electrolytes to achieve the desired performance.
Because testing methods and electrolytes significantly impact battery performance, changing the testing method or electrolyte may degrade electrode performance. Please verify this information before purchasing.
Electrode Sheet Technical Data Sheet (SC02XX - Si/C 420 Electrode)
| Parameter | Specification |
|---|---|
| Slurry Areal Density (mg/cm²) | 7.25 |
| Electrode Sheet Size | 10 × 10 cm |
| Current Collector Thickness (μm) | 9 (Carbon-coated Cu foil) |
| Active Material Ratio | 95.00% |
| Compacted Density (g/cc) | 1.10 (Not compacted; value needs self-calculation) |
| Active Material | Si/C 1800 (5%) + Graphite (95%) |
| Recommended Electrolyte | KLD-Si01 |
| Electrode Name | Si/C 420 Electrode |
| Electrode Code | SC02XX |
| Specific Capacity (mAh/g) | 420 (0.005–2.000 V) |
| Areal Capacity (mAh/cm²) | 1.9 |
| Coating Areal Density (mg/cm²) | 4.80 (Tolerance ±2.0%) |
Usage Recommendations
-
If the electrode is not compacted, it should be compacted before punching and baking. (Reference minimum value above for compacted density.)
-
Baking conditions: 85–105°C for 4 hours.
If vacuum baking, replace the air twice. -
Active material mass should be weighed for each circular electrode individually for accurate calculation.
Compatible Full Cell Electrode Models (N/P Ratio ≈ 1.09)
SY13XX, SY25XX, SY33XX, LF06XX, LC02XX
Test Conditions
-
Ambient temperature: 25°C, rest for 4 h
-
Discharge: 0.10C / 0.09C / 0.08C / ... / 0.01C (constant current) to 0.005 V
-
Rest for 3 min
-
Charge: 0.1C (constant current) to 2.00 V
-
Rest for 3 min
Shelf Life
-
6 months in vacuum-sealed storage
-
Use within 1 month after opening
Capacity Measurement Conditions
-
25°C
-
0.10 / 0.09 / 0.08 / 0.07 / 0.06 / 0.05 / 0.04 / 0.03 / 0.02 / 0.01 C DC discharge to 0.005 V
-
0.1 C CC charge to 2.00 V
Need R&D Support?
Browse key product categories and connect battery materials with Canrd's R&D services for testing, fabrication, and project support.
Experimental Materials
CategoryCathode, anode, electrolyte, separator, and other materials for battery research.
Shop cathode, anode & electrolyte materials →Lab Equipment
CategoryBattery lab equipment for pilot lines, fixtures, and testing workflows.
Browse battery lab equipment →Electrodes & Cells
CategoryCustom electrodes, dry cells, and battery cell components for R&D validation.
View custom battery electrodes & cells →Sodium Electrolyte
CategorySodium-ion electrolyte options for sodium battery research and validation.
Shop sodium battery electrolytes →R&D Services
ServiceFull-chain battery R&D services from material evaluation to cell fabrication and failure analysis.
Explore Canrd R&D services →Material Evaluation
ServiceCharacterization, electrochemical testing, and compatibility evaluation for battery materials.
Evaluate your battery materials →Electrode Fabrication
ServiceCustom electrode sheets and rolls based on your target chemistry and process needs.
Request electrode fabrication →Cell Fabrication
ServiceDry cells, assembled cells, and custom-format cell builds for R&D validation.
Build custom research cells →Contact
PageAsk Canrd to match products, materials, and services for your project.
Get product and R&D support →