Details
High-voltage lithium nickel manganese oxide, with a voltage up to 4.8V and a high voltage plateau.


Due to the material's unique characteristics, the first 5 cycles require activation at 0.1C.
Packaging requirements: Inner layer sealed plastic bottle, outer layer aluminum-plastic film sealed.
Storage requirements: Sealed, store in a cool, dry place.
Material requires vacuum sealing for storage.
Material is hygroscopic; humidity must be controlled throughout the sheet preparation process.
Electrolyte used for testing: Ternary electrolyte (KLD-1230C).