Details
| NO. | Electrode Name | Model | Main Material | Active Material Capacity (mAh/g) | Loading | Areal Density (mg/cm²) | Areal Capacity (mAh/cm²) |
| 1 | NCM811 Electrode | SY33 | NCM811 Single Crystal | 188 | 94.5% | 9.20 | 1.63 |
| 2 | NCM811 Electrode | SY34 | — | 188 | 94.5% | 21.50 | 3.82 |
| 3 | NCM622 Electrode | SY25 | NCM622 Single Crystal-B | 168 | 96.7% | 10.00 | 1.62 |
| 4 | NCM622 Electrode | SY24 | — | 168 | 96.7% | 21.60 | 3.51 |
| 5 | NCM523 Electrode | SY15 | NCM523 | 165 | 94.0% | 19.70 | 3.06 |
| 6 | NCM523 Electrode | SY13 | NCM523 | 165 | 94.0% | 10.50 | 1.63 |
| 7 | LCO Electrode | LC02 | High Voltage Lithium Cobalt Oxide-Z-4.45V | 178 | 96.4% | 10.00 | 1.72 |
| 8 | LRM Electrode | FL01 | Lithium-rich Manganese-based-E | 280 | 95.0% | 5.96 | 1.59 |
| 9 | Graphite Electrode | SM02 | Natural Graphite (Standard)-A | 340 | 95.7% | 5.80 | 1.89 |
| 10 | Fast Charging Graphite Electrode | SM04 | Fast Charging Graphite-B | 350 | 96.7% | 5.60 | 1.90 |
| 11 | Silicon Carbon Electrode | SC02 | Silicon Carbon Anode 1800 (Porous Carbon Deposited Silicon) | 420 | 95.0% | 4.80 | 1.92 |
| 12 | NFM Electrode | NT02 | Sodium Nickel Iron Manganese Oxide | 127 | 95.5% | 12.27 | 1.49 |
| 13 | NFM Electrode | NT03 | — | 127 | 95.5% | 8.00 | 0.97 |
| 14 | Hard Carbon Electrode | YT02 | Imported Hard Carbon (5 μm) | 300 | 95.5% | 6.00 | 1.72 |
| 15 | LFP Electrode | LF07 | Lithium Iron Phosphate (High Compaction Density) | 150 | 91.5% | 12.30 | 1.69 |
| 16 | LNMO Electrode | NM01 | High Voltage Lithium Nickel Manganese Oxide-B | 130 | 96.0% | 7.50 | 2.00 |
| 17 | NFPP Electrode | NF01 | Sodium Iron Phosphate Pyrophosphate | 100 | 93.5% | 15.30 | 1.43 |
| 18 | Vanadium Pentoxide Electrode | VO02 | Vanadium Pentoxide | 300 | 80.0% | 5.00 | 1.20 |
| 19 | Manganese Dioxide Electrode | MO02 | Modified Manganese Dioxide (γ-phase) - Long Cycle | 100 | 90.0% | 10.00 | 0.90 |
| 20 | Zinc Negative Electrode | ZA01 | Pure Zinc Powder / Alloy Zinc Powder | / | 70.0%-96.0% | 5.0–15.0 | / |
| 21 | Super capacitor dry process electrode | 6M2302001 | YP50 activated carbon | / | 96.0% | 11.50 | / |
| 22 | Zinc-iodine battery electrode | ZIXX01 | iodine-based active substances | / | / | 20~80 | / |
MOQ for Custom Small Electrode Sheets: 10*10cm/pcs, 5cs/pack, 1pack
To place an order or request a quotation, please Contact Us.
This product must be tested in accordance with the test methods, electrolyte and other specifications recommended by CANRD to achieve its designated performance.
Since test methods, electrolyte and other factors exert significant impacts on battery performance, any modification to the test method or electrolyte may degrade the electrode performance. Please verify this information carefully before purchase.
The battery can be assembled under ambient conditions and does not require assembly inside a glove box.
Front and back sides of the electrode sheet: see figure below:

| Electrode Name | Manganese Dioxide Electrode |
|---|---|
| Electrode No. | MO02 |
| Active Material | Modified Manganese Dioxide (γ-phase) - Long Cycle |
| Electrode Size (cm) | 10*10 |
| Active Material Ratio / Loading | 90.0% |
| Specific Capacity of Active Material (mAh/g) | 100 (1.0–1.9 V) |
| Coating Loading (mg/cm²) | 10.00 |
| Areal Capacity (mAh/cm²) | 0.90 |
| Current Collector Thickness (μm) | 20 (Stainless Steel Foil) |
| Current Collector Loading (mg/cm²) | 17.00 |
| Compaction Density (g/cc) | 1.50 |
| Recommended Separator | Separator for Zinc-Ion Battery: Sulfurized Composite Separator (Single Sulfurization) |
| Recommended Electrolyte | Zinc-Ion Electrolyte, 2 M ZnSO₄ |
| Matching Full-Cell Electrode Model (N/P ratio) | Zinc-Ion Battery Anode Electrode (Zn Anode ZA01) |
| Shelf Life | 6 months (store under vacuum packaging); use within 1 month after opening |
| Test Conditions | 25°C ambient, 0.1/0.1 A/g, 1.0–1.9 V |
| Test Condition Description | 25°C ambient, rest for 4 h
|
| Usage Suggestions | 1. Pre-treatment before electrode assembly: overnight drying at 110°C
|

Product Description & Recommendations
- Store under vacuum or double-seal with zipper bags inside a glove box. This is especially critical for high-nickel and sodium-ion cathode materials. Improper storage will lead to increased internal resistance of batteries.
- The electrode sheets are uncalendared. Calendering shall be performed according to the recommended compaction density.
- The coating areal loading shall be determined by actual weighing. The coating areal loading excludes the current collector.
- Formula for calculating the mass of active material by actual weighing: Mass of active material (mg) = (Weight of disc (mg) − Current collector areal loading (mg/cm²) × Area of disc (cm²)) × Active material ratio
- Theoretical mass of active material (mg) = Coating areal loading (mg/cm²) × Active material ratio × Area of disc (cm²)
- Theoretical areal capacity (mAh/cm²) = Coating areal loading (mg/cm²) × Active material ratio × Specific capacity (mAh/g) ÷ 1000
- Specific capacity is calculated based on the actual weighed mass of active material. There are tolerances in coating areal loading; actual weighing shall prevail.
- Creases: Single-sided electrodes tend to curl after calendering. Flattening for packaging may cause creases.
Packaging, Transportation and Storage
Packaging Requirement: Vacuum-sealed with aluminum plastic film, packed in a plastic bag on the outer layer. Storage Requirement: Keep sealed and store in a cool and dry place.
자주 묻는 질문
검색하거나 일반적인 질문을 찾아보며 빠르게 답변을 확인하세요

R&D 지원이 필요하신가요?
주요 제품 카테고리를 확인하고 배터리 소재를 Canrd R&D 서비스와 연결하세요.
실험 소재
카테고리배터리 연구용 양극, 음극, 전해액, 분리막 및 기타 소재.
양극, 음극 및 전해액 소재 보기 →실험 장비
카테고리파일럿 라인, 지그 및 테스트 워크플로용 배터리 실험 장비.
배터리 실험 장비 보기 →전극 및 셀
카테고리R&D 검증을 위한 맞춤 전극, 드라이 셀 및 배터리 셀 부품.
맞춤 배터리 전극 및 셀 보기 →나트륨 전해액
카테고리나트륨 배터리 연구 및 검증을 위한 나트륨 이온 전해액 옵션.
나트륨 배터리 전해액 보기 →R&D 서비스
서비스소재 평가부터 셀 제작 및 고장 분석까지 전주기 배터리 R&D 서비스.
Canrd R&D 서비스 살펴보기 →소재 평가
서비스배터리 소재의 특성 분석, 전기화학 테스트 및 호환성 평가.
배터리 소재 평가하기 →전극 제작
서비스목표 화학계와 공정 요구에 맞춘 맞춤 전극 시트 및 롤.
전극 제작 요청하기 →셀 제작
서비스R&D 검증을 위한 드라이 셀, 조립 셀 및 맞춤 셀 형식.
맞춤 연구 셀 제작하기 →문의
페이지Canrd가 프로젝트에 맞는 제품, 소재 및 서비스를 연결해 드립니다.
제품 및 R&D 지원 받기 →