Lithium-ion Battery Cathode Electrode Sheet (NCM811 Lithium Nickel Cobalt Manganese Oxide SY34)
Lithium-ion Battery Cathode Electrode Sheet (NCM811 Lithium Nickel Cobalt Manganese Oxide SY34)
Lithium-ion Battery Cathode Electrode Sheet (NCM811 Lithium Nickel Cobalt Manganese Oxide SY34)
Lithium-ion Battery Cathode Electrode Sheet (NCM811 Lithium Nickel Cobalt Manganese Oxide SY34)
Lithium-ion Battery Cathode Electrode Sheet (NCM811 Lithium Nickel Cobalt Manganese Oxide SY34)

Lithium-ion Battery Cathode Electrode Sheet (NCM811 Lithium Nickel Cobalt Manganese Oxide SY34)

$75.51
Model:
SY34XX
item_No
Specifications
Price
SY34XX
Single side (5 sheets/pack) (not rolled)
$75.51

Details

This NCM811 electrode sheet (SY34XX) is developed for advanced lithium-ion battery research, featuring a single-crystal nickel-cobalt-manganese (NCM811) active material with a high active material ratio of 94.5%. The electrode, coated on a 12 µm aluminum foil current collector, delivers a specific capacity of 188 mAh/g (3.00–4.30V) and an areal capacity of 3.82 mAh/cm², with a coating areal density of 21.50 mg/cm². Available in both roll-pressed and unrolled configurations, the unrolled sheets require custom compaction. Designed for full-cell testing with the recommended electrolyte KLD-1230C, this electrode supports a 6-month shelf life under vacuum sealing and is typically used in laboratory-scale coin cells or small pouch cells. Its high nickel content and single-crystal structure make it suitable for studying high-energy-density cathode performance.

Current collector areal density (mg/cm²) 3.40 
Electrode size 10*10
Current collector thickness (µm) 12 (Aluminum foil)
Active material ratio 94.5%
Compatible electrode type for full cells (N/P ratio) None (Customization is available upon request).
Pack density (g/cc) 2.50-3.35 (Compaction value not provided for unrolled electrode sheets; calculate it yourself)
Active material Nickel-Cobalt-Manganese NCM811 (Single Crystal)
Shelf life 6 months (vacuum sealed). Use within one month of opening.
Recommended electrolyte KLD-1230C
Electrode name NCM811 electrode sheet
Electrode number SY34XX
Active material specific capacity (mAh/g) 188(3.00-4.30V)
Test conditions description At room temperature (25℃), let stand for 4 hours, charge at a 0.1C rate (constant current) to 4.30V, charge at 4.30V constant voltage to 0.02C, let stand for 3 minutes, discharge at a 0.1C rate (constant current) to 3.00V, and let stand for 3 minutes.
Test condition  At room temperature (25℃), 0.1/0.1C, 2.50-4.20V
Areal capacity (mAh/cm²) 3.82 
Coating areal density (mg/cm²) 21.50 (tolerance ±2.0%)
Usage recommendations

1. If the electrode sheet is not rolled, it generally needs to be rolled before punching and baking (the compaction density can be referenced from the minimum value in the "Compaction Density" column of this table);

2. Baking conditions: 85-105℃ for 4 hours (if vacuum baking, two air changes are required);
3. The areal density needs to be determined based on the actual weight of each small disc.