Details
| Canrd | 10*10cm | 5 sheets/pack | Coating | ||||
| NO. | Electrode Name | Model | Main Material | Active Material Capacity (mAh/g) | Loading | Areal Density (mg/cm²) | Areal Capacity (mAh/cm²) |
| 1 | NCM811 Electrode | SY33 | NCM811 Single Crystal | 188 | 94.50% | 9.20 | 1.63 |
| 2 | NCM811 Electrode | SY34 | — | 188 | 94.50% | 21.50 | 3.82 |
| 3 | NCM622 Electrode | SY25 | NCM622 Single Crystal-B | 168 | 96.70% | 10.00 | 1.62 |
| 4 | NCM622 Electrode | SY24 | — | 168 | 96.70% | 21.60 | 3.51 |
| 5 | NCM523 Electrode | SY15 | NCM523 | 165 | 94.00% | 19.70 | 3.06 |
| 6 | NCM523 Electrode | SY13 | NCM523 | 165 | 94.00% | 10.50 | 1.63 |
| 7 | LCO Electrode | LC02 | High Voltage Lithium Cobalt Oxide-Z-4.45V | 178 | 96.40% | 10.00 | 1.72 |
| 8 | LRM Electrode | FL01 | Lithium-rich Manganese-based-E | 280 | 95.00% | 5.96 | 1.59 |
| 9 | Graphite Electrode | SM02 | Natural Graphite (Standard)-A | 340 | 95.70% | 5.80 | 1.89 |
| 10 | Fast Charging Graphite Electrode | SM04 | Fast Charging Graphite-B | 350 | 96.70% | 5.60 | 1.90 |
| 11 | Silicon Carbon Electrode | SC02 | Silicon Carbon Anode 1800 (Porous Carbon Deposited Silicon) | 420 | 95.00% | 4.80 | 1.92 |
| 12 | NFM Electrode | NT02 | Sodium Nickel Iron Manganese Oxide | 127 | 95.50% | 12.27 | 1.49 |
| 13 | NFM Electrode | NT03 | — | 127 | 95.50% | 8.00 | 0.97 |
| 14 | Hard Carbon Electrode | YT02 | Imported Hard Carbon (5 μm) | 300 | 95.50% | 6.00 | 1.72 |
| 15 | LFP Electrode | LF07 | Lithium Iron Phosphate (High Compaction Density) |
150 | 91.50% | 12.30 | 1.69 |
| 16 | LNMO Electrode | NM01 | High Voltage Lithium Nickel Manganese Oxide-B | 130 | 96.00% | 7.50 | 2.00 |
| 17 | NFPP Electrode | NF01 | Sodium Iron Phosphate Pyrophosphate | 100 | 93.50% | 15.30 | 1.43 |
| 18 | Vanadium Pentoxide Electrode | VO02 | Vanadium Pentoxide | 300 | 80.00% | 5.00 | 1.20 |
| 19 | Manganese Dioxide Electrode | MO02 | Modified Manganese Dioxide (γ-phase) - Long Cycle | 100 | 90.00% | 10.00 | 0.90 |
| 20 | Zinc Negative Electrode | ZA01 | Pure Zinc Powder / Alloy Zinc Powder | / | 70.0%–96.0% | 5.0–15.0 | / |
| 21 | Super capacitor dry process electrode | 6M2302001 | YP50 activated carbon | / | 96.0% | 11.50 | / |
| 22 | Zinc–iodine battery electrode | ZIXX01 | iodine-based active substances | / | / | 20-80 | / |
MOQ for Custom Small Electrode Sheets: 10*10cm/pcs,5cs/pack,1pack
To place an order or request a quotation, please Contact Us.
Because it is a single-sided electrode, there will be a curl after rolling, so the shipped roller-pressed electrode has controlled and compacted to ensure that the electrode is not rolled;
Rolling can improve the compacting density of the electrode, improve the electronic conductivity of the electrode, and improve the bonding.
1. The electrode should be rolled before use, and the customer needs to arrange the rolling pressure by himself to purchase the electrode that has not been rolled;
2. The surface density shall be determined according to the actual weighing results;
3. Before putting it in the glove box, the punched electrode needs to be vacuum baked at a temperature of 105 °C for 4 hours;
4. This electrode can be matched with our YT0101 anode electrode; 5. The density of the coating surface does not include the current collector;
6. Theoretical surface capacity mAh/cm2 = coating surface density mg/cm2 * proportion of active substance * gram capacity mAh/g÷1000;
7. The amount of theoretical active substance (mg) = coating surface density mg/cm2 * proportion of active substance * small disc area cm2;
8. The actual weighing calculates the amount of active substance (mg) = (weight of small disc mg - current collector surface density mg/cm2 * small disc area cm2) * proportion of active substance, and calculates the gram capacity according to the amount of active substance actually weighed, due to the tolerance of the density of the coating surface, the actual weighing shall prevail.

This product must be tested in accordance with the test methods and electrolytes recommended by Coulter to achieve the corresponding performance.Since the test method and electrolyte have a great influence on the performance of the battery, any change in the test method or electrolyte may reduce the performance of the pole piece; be sure to check this information before purchasing.
| Surface density of the current collector (mg/cm2) | 3.3 |
| Current collector thickness (µm) | 12 (aluminum foil) |
| Electrode size | 10*10cm |
| active ingredient ratio | 95.50% |
| Electrode types compatible with full-cell batteries (N/P ratio) | YT02XX(1.16) |
| Compacted density (g/cc) | 2.00-2.50 (Compaction value not provided for unrolled electrode sheets; calculate it yourself) |
| Active materials | Sodium nickel iron manganate |
| Shelf life | Store for six months (vacuum sealed); use within one month of opening. |
| Recommended electrolyte | KLD-NC06 |
| Extreme film name | Sodium-nickel iron manganese oxide electrode |
| Electrode Number | NT02XX |
| Active material specific capacity (mAh/g) | 120 (2.00-4.00V) |
| Test Conditions Description | At room temperature (25℃), let stand for 4 hours, charge at a 0.1C rate (constant current) to 4.00V, charge at 4.00V constant voltage to 0.02C, let stand for 3 minutes, discharge at a 0.1C rate (constant current) to 2.00V, and let stand for 3 minutes. |
| Test conditions | Normal temperature 25℃, 0.1/0.1C, 2.00-4.00V |
| Surface capacity (mAh/cm2) | 1.49 |
| Coating areal density (mg/cm2) | 12.27 (tolerance is ±2.0%) |
| Usage Recommendations |
1. If the electrode sheet is not rolled, it generally needs to be rolled before punching and baking (the compaction density can be referenced from the minimum value in the "Compaction Density" column of this table); 2. Baking conditions: 85-105℃ for 4 hours (if vacuum baking, it needs to be ventilated twice); 3. The mass of active material needs to be determined according to the actual weight of each small disc. |

よくある質問
検索または一般的な質問を閲覧して、素早く回答を見つける

R&Dサポートが必要ですか?
主要な製品カテゴリを確認し、バッテリー材料をCanrdのR&Dサービスにつなげます。
実験材料
カテゴリバッテリー研究向けの正極、負極、電解液、セパレーターなど。
正極・負極・電解液材料を見る →実験装置
カテゴリパイロットライン、治具、試験ワークフロー向けのバッテリー実験装置。
バッテリー実験装置を見る →電極とセル
カテゴリR&D検証向けのカスタム電極、乾燥セル、セル部材。
カスタムバッテリー電極とセルを見る →ナトリウム電解液
カテゴリナトリウム電池研究と検証向けのナトリウムイオン電解液。
ナトリウム電池電解液を見る →R&Dサービス
サービス材料評価からセル作製、故障解析までの一貫したバッテリーR&Dサービス。
Canrd R&Dサービスを見る →材料評価
サービスバッテリー材料の特性評価、電気化学試験、適合性評価。
バッテリー材料を評価する →電極作製
サービス対象化学系とプロセスに合わせたカスタム電極シートやロール。
電極作製を依頼する →セル作製
サービスR&D検証向けの乾燥セル、組立セル、カスタムセル形式。
カスタム研究セルを作製する →お問い合わせ
ページCanrdが製品、材料、サービスをプロジェクトに合わせて提案します。
製品とR&Dサポートを受ける →