Physical Properties:
| Test Item | Unit | Specification Range | Test Result | |
| Appearance | / | Black powder | Visual inspection | |
| Particle Size | Dn10 | μm | ≥3.0 | 3.6 |
| Dv01 | μm | ≥3.0 | 3.5 | |
| Dv10 | μm | 5.0 ± 0.5 | 4.9 | |
| Dv50 | μm | 8.0 ± 0.5 | 8.1 | |
| Dv90 | μm | ≤18.0 | 13 | |
| BET Specific Surface Area | m²/g | ≥1900 | 1923 | |
| Pore Volume | cm³/g | 0.90 ± 0.03 | 0.87 | |
| Micropore Fraction | % | >85 | 91.3 | |
| Single-Point Average Pore Diameter | nm | <2.0 | 1.72 | |
| Tap Density | g/cm³ | ≥0.30 | 0.43 | |
| Ash Content | % | ≤0.3 | 0.02 | |
| Moisture Content | % | ≤1.0 | 0.413 | |
| pH | / | 7.5 ± 1.5 | 7.2 | |
| Impurity Content | Fe | ppm | ≤100 | 15.58 |
| Co | ppm | ≤20 | 0.35 | |
| Cr | ppm | ≤10 | 0.71 | |
| Ni | ppm | ≤50 | 1.8 | |
| Cu | ppm | ≤10 | 0.35 | |
| Na | ppm | ≤150 | 8.66 | |
| Ca | ppm | ≤100 | 21.71 | |
| Zn | ppm | ≤25 | 3.35 | |
| Magnetic Substances | ppm | ≤1.0 | 0.23 | |
SEM:



Packaging, Transportation, and Storage:
Store the product in a clean, cool, and dry environment at ambient temperature (temperature ≤45 °C; relative humidity ≤90% RH).
Product Instructions and Recommendations:
When kept in sealed packaging and stored in a cool, dry place, the shelf life is six months.
R&Dサポートが必要ですか?
主要な製品カテゴリを確認し、バッテリー材料をCanrdのR&Dサービスにつなげます。
実験材料
カテゴリバッテリー研究向けの正極、負極、電解液、セパレーターなど。
正極・負極・電解液材料を見る →実験装置
カテゴリパイロットライン、治具、試験ワークフロー向けのバッテリー実験装置。
バッテリー実験装置を見る →電極とセル
カテゴリR&D検証向けのカスタム電極、乾燥セル、セル部材。
カスタムバッテリー電極とセルを見る →ナトリウム電解液
カテゴリナトリウム電池研究と検証向けのナトリウムイオン電解液。
ナトリウム電池電解液を見る →R&Dサービス
サービス材料評価からセル作製、故障解析までの一貫したバッテリーR&Dサービス。
Canrd R&Dサービスを見る →材料評価
サービスバッテリー材料の特性評価、電気化学試験、適合性評価。
バッテリー材料を評価する →電極作製
サービス対象化学系とプロセスに合わせたカスタム電極シートやロール。
電極作製を依頼する →セル作製
サービスR&D検証向けの乾燥セル、組立セル、カスタムセル形式。
カスタム研究セルを作製する →お問い合わせ
ページCanrdが製品、材料、サービスをプロジェクトに合わせて提案します。
製品とR&Dサポートを受ける →