This product is a polycrystalline nickel cobalt manganese (NCM523) precursor developed for use in lithium-ion battery cathode materials. As a non-lithiated intermediate, it contains no inherent electrochemical capacity; its final performance is established during calcination, where lithium salts and additives are introduced under controlled mixing and sintering conditions. The precursor’s properties—such as particle morphology and compositional homogeneity—directly influence the electrochemical characteristics of the resulting NCM523 cathode. It is commonly employed in research and development settings for synthesizing high-nickel ternary cathode materials, where precise processing optimization is required. Supplied as a sealed powder in quantities from 20 g to 1 kg, it should be stored away from humidity, high temperatures, and strong oxidizers to maintain stability over a one-year shelf life.

Product Description

Nickel Cobalt Manganese (NCM523) Precursor – Polycrystalline

1、The precursor itself does not contain lithium ions, therefore it has no specific capacity or efficiency data.

2、During calcination into the final cathode material, lithium salts and additives must be introduced. The amounts, mixing method, and sintering process will significantly affect the electrochemical performance.

3、As performance strongly depends on processing conditions, no fixed electrochemical specifications can be provided.

Packaging, Transportation & Storage

1、Packaging: Inner sealed plastic bottle, outer aluminum-plastic laminate.

2、Storage: Keep sealed, away from strong oxidizers. Avoid humidity and high temperature.

3、Shelf life: 1 year from the date of production.