Details
This NCM622 cathode electrode sheet is designed for advanced lithium-ion battery research, featuring single-crystal nickel-cobalt-manganese (NCM622-C) active material. The electrode is optimized for use with Canrd-recommended testing protocols and specific electrolytes, such as 622 cutoff or ternary electrolyte KLD-1230C, to ensure reliable electrochemical performance. Proper handling is critical: storage requires vacuum or doubled sealed bags to prevent moisture-induced degradation, and the sheet requires rolling within the suggested compactness range to avoid fold lines. Typical applications include coin-cell and pouch-cell fabrication for evaluating cathode performance under controlled conditions. The product is available in rolled or unrolled formats, with customized options, and is intended for users familiar with standardized electrode preparation procedures.
| Canrd | 10*10cm | 5 sheets/pack | Coating | ||||
| NO. | Electrode Name | Model | Main Material | Active Material Capacity (mAh/g) | Loading | Areal Density (mg/cm²) | Areal Capacity (mAh/cm²) |
| 1 | NCM811 Electrode | SY33 | NCM811 Single Crystal | 188 | 94.50% | 9.20 | 1.63 |
| 2 | NCM811 Electrode | SY34 | — | 188 | 94.50% | 21.50 | 3.82 |
| 3 | NCM622 Electrode | SY25 | NCM622 Single Crystal-B | 168 | 96.70% | 10.00 | 1.62 |
| 4 | NCM622 Electrode | SY24 | — | 168 | 96.70% | 21.60 | 3.51 |
| 5 | NCM523 Electrode | SY15 | NCM523 | 165 | 94.00% | 19.70 | 3.06 |
| 6 | NCM523 Electrode | SY13 | NCM523 | 165 | 94.00% | 10.50 | 1.63 |
| 7 | LCO Electrode | LC02 | High Voltage Lithium Cobalt Oxide-Z-4.45V | 178 | 96.40% | 10.00 | 1.72 |
| 8 | LRM Electrode | FL01 | Lithium-rich Manganese-based-E | 280 | 95.00% | 5.96 | 1.59 |
| 9 | Graphite Electrode | SM02 | Natural Graphite (Standard)-A | 340 | 95.70% | 5.80 | 1.89 |
| 10 | Fast Charging Graphite Electrode | SM04 | Fast Charging Graphite-B | 350 | 96.70% | 5.60 | 1.90 |
| 11 | Silicon Carbon Electrode | SC02 | Silicon Carbon Anode 1800 (Porous Carbon Deposited Silicon) | 420 | 95.00% | 4.80 | 1.92 |
| 12 | NFM Electrode | NT02 | Sodium Nickel Iron Manganese Oxide | 127 | 95.50% | 12.27 | 1.49 |
| 13 | NFM Electrode | NT03 | — | 127 | 95.50% | 8.00 | 0.97 |
| 14 | Hard Carbon Electrode | YT02 | Imported Hard Carbon (5 μm) | 300 | 95.50% | 6.00 | 1.72 |
| 15 | LFP Electrode | LF07 | Lithium Iron Phosphate (High Compaction Density) |
150 | 91.50% | 12.30 | 1.69 |
| 16 | LNMO Electrode | NM01 | High Voltage Lithium Nickel Manganese Oxide-B | 130 | 96.00% | 7.50 | 2.00 |
| 17 | NFPP Electrode | NF01 | Sodium Iron Phosphate Pyrophosphate | 100 | 93.50% | 15.30 | 1.43 |
| 18 | Vanadium Pentoxide Electrode | VO02 | Vanadium Pentoxide | 300 | 80.00% | 5.00 | 1.20 |
| 19 | Manganese Dioxide Electrode | MO02 | Modified Manganese Dioxide (γ-phase) - Long Cycle | 100 | 90.00% | 10.00 | 0.90 |
| 20 | Zinc Negative Electrode | ZA01 | Pure Zinc Powder / Alloy Zinc Powder | / | 70.0%–96.0% | 5.0–15.0 | / |
| 21 | Super capacitor dry process electrode | 6M2302001 | YP50 activated carbon | / | 96.0% | 11.50 | / |
| 22 | Zinc–iodine battery electrode | ZIXX01 | iodine-based active substances | / | / | 20-80 | / |
MOQ for Custom Small Electrode Sheets: 10*10cm/pcs,5cs/pack,1pack
To place an order or request a quotation, please Contact Us.
Storage Conditions (Vacuum storage or double-layered sealing in self-sealing bags within the glove box, especially for high-nickel and sodium-positive electrode materials; improper storage might lead to increased internal resistance in batteries).
Fold Lines: Single-sided cathode sheets tend to curl after rolling, leading to potential fold lines when flattened for packaging.
Materials used in this cathode sheet: Nickel Cobalt Manganese NCM622-C (single crystal). Electrolytes used during testing: 622 cut-off electrolyte; ternary electrolyte (KLD-1230C).
Rolling of cathode sheets required (recommend pressing within the lower range of the suggested compactness for the respective cathode sheets), cathode sheet baking conditions at 105°C for 4 hours, 8 hours of static placement after injection, and post-charge sealing pressure of 1300 psi for the positive electrode cathode sheet after constant current charging at 0.02C.
This product must be tested according to Canrd recommended testing methods and electrolytes to achieve the desired performance.
Because testing methods and electrolytes significantly impact battery performance, changing the testing method or electrolyte may degrade electrode performance. Please verify this information before purchasing.


よくある質問
検索または一般的な質問を閲覧して、素早く回答を見つける

R&Dサポートが必要ですか?
主要な製品カテゴリを確認し、バッテリー材料をCanrdのR&Dサービスにつなげます。
実験材料
カテゴリバッテリー研究向けの正極、負極、電解液、セパレーターなど。
正極・負極・電解液材料を見る →実験装置
カテゴリパイロットライン、治具、試験ワークフロー向けのバッテリー実験装置。
バッテリー実験装置を見る →電極とセル
カテゴリR&D検証向けのカスタム電極、乾燥セル、セル部材。
カスタムバッテリー電極とセルを見る →ナトリウム電解液
カテゴリナトリウム電池研究と検証向けのナトリウムイオン電解液。
ナトリウム電池電解液を見る →R&Dサービス
サービス材料評価からセル作製、故障解析までの一貫したバッテリーR&Dサービス。
Canrd R&Dサービスを見る →材料評価
サービスバッテリー材料の特性評価、電気化学試験、適合性評価。
バッテリー材料を評価する →電極作製
サービス対象化学系とプロセスに合わせたカスタム電極シートやロール。
電極作製を依頼する →セル作製
サービスR&D検証向けの乾燥セル、組立セル、カスタムセル形式。
カスタム研究セルを作製する →お問い合わせ
ページCanrdが製品、材料、サービスをプロジェクトに合わせて提案します。
製品とR&Dサポートを受ける →