Details
Use Method:
It was mixed with water in a certain proportion and treated with ultrasound (recommended for a cell grinder) (power: 300W; time: 15 minutes) to prepare an aqueous solution of graphene oxide.
This product was prepared using the modified Hummers method. It is rich in a large number of oxygen-containing functional groups and has good hydrophilicity. A stable electrostatic double layer can be formed in water, making it form a stable and dispersed solution. Compared with ordinary graphite oxide, oxygen-containing functional groups are richer, chemically active, and more interlayered, making it easier to peel off. This product is prepared in small batches in the laboratory, with excellent performance, stable quality and high cost performance, and is specially used for scientific research experiments.
Applications:
1. Electrochemical energy storage (superpower, lithium, etc.)
2. Conductive inks
3. Antistatic material
4. Composites
5. Electromagnetic protective materials
6. Thermal management materials
7. Anticorrosive coatings
8. Carriers (catalysts, drugs)
9. Sensors
10. Adsorbent materials

Graphite oxide powder SEM image

R&Dサポートが必要ですか?
主要な製品カテゴリを確認し、バッテリー材料をCanrdのR&Dサービスにつなげます。
実験材料
カテゴリバッテリー研究向けの正極、負極、電解液、セパレーターなど。
正極・負極・電解液材料を見る →実験装置
カテゴリパイロットライン、治具、試験ワークフロー向けのバッテリー実験装置。
バッテリー実験装置を見る →電極とセル
カテゴリR&D検証向けのカスタム電極、乾燥セル、セル部材。
カスタムバッテリー電極とセルを見る →ナトリウム電解液
カテゴリナトリウム電池研究と検証向けのナトリウムイオン電解液。
ナトリウム電池電解液を見る →R&Dサービス
サービス材料評価からセル作製、故障解析までの一貫したバッテリーR&Dサービス。
Canrd R&Dサービスを見る →材料評価
サービスバッテリー材料の特性評価、電気化学試験、適合性評価。
バッテリー材料を評価する →電極作製
サービス対象化学系とプロセスに合わせたカスタム電極シートやロール。
電極作製を依頼する →セル作製
サービスR&D検証向けの乾燥セル、組立セル、カスタムセル形式。
カスタム研究セルを作製する →お問い合わせ
ページCanrdが製品、材料、サービスをプロジェクトに合わせて提案します。
製品とR&Dサポートを受ける →