Details
The material needs to be vacuum sealed for storage
The material is prone to water absorption, and humidity control is required throughout the entire production process
The electrolyte used during testing is NCM electrolyte (KLD-1230C)
Baking conditions for electrode: Bake at 85 ℃ for 4 hours
Note: Production has ceased; products will be removed from shelves once sold out.
Lithium ion battery cathode, Ni, Co, Mn NCM material, excellent cycling performance
Physical and chemical properties

Half battery test




SEM

Remarks: CC rate charging, DC rate discharging, CV constant voltage charging