MA-EN-CA-008601
20g
$60.41

Details

Lithium-ion battery ternary cathode material, solid electrolyte coated NCM613 (polycrystalline), coated material LATP, coated amount ~ 0.5%

Physical and chemical properties
Serial Number Test items Units Specifications Measured results Inspection method or instrument
1 Chemical composition Ni (mol%) 60.0±1.0 60.45 ICP
2 Li (wt%) 7.5±0.5 7.47
3 Co (mol%) 10.0±1.0 10.12
4 Mn (mol%) 30.0±1.0 29.32
5 Fe (ppm) ≤15 9.1
6 Cu (ppm) ≤10 0.0
7 S (ppm) ≤1000 672.0
8 Ca (ppm) ≤100 10.0
9 Na (ppm) ≤200 82.0
10 Metal impurities (ppb) ≤40 8.0
11 Physical Properties Particle size distribution D10 (μm) 2.0±1.0 2.021 Laser particle size analyzer
12 D50 (μm) 4.0±1.0 3.872
13 D90 (μm) 7.0±2.0 7.132
14 BET (m2/g) 0.8±0.2 0.92 Automatic specific surface and porosity analyzer
15 TD (g/cm3) 2.4±0.3 2.42 Tweak density gauge
16 pH / 11.4±0.5 11.43 pH meter
17 Moisture (ppm) ≤400.0 128.0 Moisture Analyzer
18 Electrochemical Performance First discharge capacity (mAh/g) ≥170.0 186.2 CR2032
0.1/0.1C(4.45-3.00V)
19 First Time Efficiency (%) ≥85.0 87.7

Product Description, Recommendations

Material to be vacuum sealed

The electrolyte used in the test is: KLD-1376

pole piece baking conditions: 85-105 ℃ baking 4h