Details
The material needs to be vacuum sealed for storage
The material is prone to water absorption, and humidity control is required throughout the entire production process
The electrolyte used during testing is sodium ion electrolyte KLD-NC06
Baking conditions for electrode: Bake at 105 ℃ for 4 hours
Sodium ion cathode electrode material, polyanion type, excellent rate performance, excellent cycling performance
Physical and chemical properties

Half battery test:




CC rate charging, DC rate discharge, CV constant voltage charging