Sodium iron phosphate pyrophosphate
Sodium iron phosphate pyrophosphate
Sodium iron phosphate pyrophosphate

Sodium iron phosphate pyrophosphate

$15.10
Model:
MA-EN-CA-0010
item_No
Specifications
Price
MA-EN-CA-001001
20g
$15.10

Details

The material needs to be vacuum sealed for storage

The material is highly hygroscopic, so it is essential to control the dew point temperature to be ≤ -30 ℃ throughout the entire production process

The electrolyte used during testing is sodium ion electrolyte KLD-NC06

Baking conditions for electrode: Bake at 105 ℃ for 4 hours

Cathode electrode material for sodium ion batteries, polyanion type, material sensitive to moisture, excellent cycling performance

 

Physical and chemical properties

image.png

 

Half-cell testing

cf07ab819a9d86bfd44976f1b1c7c2f.jpg

9b948b33aff216c829b6991b486d81b.jpg

b71bcbae892a06e97bdb5671b0b240f.jpg

549106bdef078e9c21d9b88111aa79e.jpg

CC-Constant current charging; CV-Constant voltage charging;DC-Constant current discharge

XRD

 

 

 

 

 

 

 

Packaging requirements: Vacuum packaging with aluminum-plastic film, outer layer packaged in plastic bags.

 

Storage requirements: Sealed, stored in a cool and dry place.