Details
The material needs to be vacuum sealed for storage
The material is highly hygroscopic, so it is essential to control the dew point temperature to be ≤ -30 ℃ throughout the entire production process
The electrolyte used during testing is sodium ion electrolyte KLD-NC06
Baking conditions for electrode: Bake at 105 ℃ for 4 hours
Cathode electrode material for sodium ion batteries, polyanion type, material sensitive to moisture, excellent cycling performance
Physical and chemical properties

Half-cell testing




CC-Constant current charging; CV-Constant voltage charging;DC-Constant current discharge
XRD

Packaging requirements: Vacuum packaging with aluminum-plastic film, outer layer packaged in plastic bags.
Storage requirements: Sealed, stored in a cool and dry place.